सिंटर्ड एनडीएफईबी चुंबक
सिंटर्ड एनडीएफईबी चुंबक भौतिक गुण | ||||||||
श्रेणी | remanence | रेव्ह. टेम्प.- कोएफ़. ब्र का | जबरदस्ती बल | आंतरिक बलपूर्वक बल | रेव्ह. टेम्प.- कोएफ़. एचसीजे का | अधिकतम. ऊर्जा उत्पाद | अधिकतम. परिचालन तापमान | घनत्व |
ब्र (केजी) | एचसीबी (आप) | एचसीजे (आप) | (बीएच) अधिकतम। (एमजीओई) | जी/सेमी³ | ||||
एन35 | 11.7-12.2 | -0.11~-0.12 | ≥10.9 | ≥12 | -0.58~-0.78 | 33-36 | 80℃ | 7.6 |
एन38 | 12.2-12.5 | -0.11~-0.12 | ≥11.3 | ≥12 | -0.58~-0.78 | 36-39 | 80℃ | 7.6 |
एन40 | 12.5-12.8 | -0.11~-0.12 | ≥11.5 | ≥12 | -0.58~-0.78 | 38-41 | 80℃ | 7.6 |
एन42 | 12.8-13.2 | -0.11~-0.12 | ≥11.5 | ≥12 | -0.58~-0.78 | 40-43 | 80℃ | 7.6 |
एन45 | 13.2-13.8 | -0.11~-0.12 | ≥11.6 | ≥12 | -0.58~-0.78 | 43-46 | 80℃ | 7.6 |
एन48 | 13.8-14.2 | -0.11~-0.12 | ≥11.6 | ≥12 | -0.58~-0.78 | 46-49 | 80℃ | 7.6 |
एन50 | 14.0-14.5 | -0.11~-0.12 | ≥10.0 | ≥12 | -0.58~-0.78 | 48-51 | 80℃ | 7.6 |
N52 | 14.3-14.8 | -0.11~-0.12 | ≥10.0 | ≥12 | -0.58~-0.78 | 50-53 | 80℃ | 7.6 |
एन33एम | 11.3-11.7 | -0.11~-0.12 | ≥10.5 | ≥14 | -0.58~-0.72 | 31-33 | 100℃ | 7.6 |
एन35एम | 11.7-12.2 | -0.11~-0.12 | ≥10.9 | ≥14 | -0.58~-0.72 | 33-36 | 100℃ | 7.6 |
एन38एम | 12.2-12.5 | -0.11~-0.12 | ≥11.3 | ≥14 | -0.58~-0.72 | 36-39 | 100℃ | 7.6 |
एन40एम | 12.5-12.8 | -0.11~-0.12 | ≥11.6 | ≥14 | -0.58~-0.72 | 38-41 | 100℃ | 7.6 |
एन42एम | 12.8-13.2 | -0.11~-0.12 | ≥12.0 | ≥14 | -0.58~-0.72 | 40-43 | 100℃ | 7.6 |
एन45एम | 13.2-13.8 | -0.11~-0.12 | ≥12.5 | ≥14 | -0.58~-0.72 | 43-46 | 100℃ | 7.6 |
एन48एम | 13.6-14.3 | -0.11~-0.12 | ≥12.9 | ≥14 | -0.58~-0.72 | 46-49 | 100℃ | 7.6 |
एन50एम | 14.0-14.5 | -0.11~-0.12 | ≥13.0 | ≥14 | -0.58~-0.72 | 48-51 | 100℃ | 7.6 |
N35H | 11.7-12.2 | -0.11~-0.12 | ≥10.9 | ≥17 | -0.58~-0.70 | 33-36 | 120℃ | 7.6 |
एन38एच | 12.2-12.5 | -0.11~-0.12 | ≥11.3 | ≥17 | -0.58~-0.70 | 36-39 | 120℃ | 7.6 |
N40H | 12.5-12.8 | -0.11~-0.12 | ≥11.6 | ≥17 | -0.58~-0.70 | 38-41 | 120℃ | 7.6 |
एन42एच | 12.8-13.2 | -0.11~-0.12 | ≥12.0 | ≥17 | -0.58~-0.70 | 40-43 | 120℃ | 7.6 |
एन45एच | 13.2-13.6 | -0.11~-0.12 | ≥12.1 | ≥17 | -0.58~-0.70 | 43-46 | 120℃ | 7.6 |
एन48एच | 13.7-14.3 | -0.11~-0.12 | ≥12.5 | ≥17 | -0.58~-0.70 | 46-49 | 120℃ | 7.6 |
एन35एसएच | 11.7-12.2 | -0.11~-0.12 | ≥11.0 | ≥20 | -0.56~-0.70 | 33-36 | 150℃ | 7.6 |
एन38एसएच | 12.2-12.5 | -0.11~-0.12 | ≥11.4 | ≥20 | -0.56~-0.70 | 36-39 | 150℃ | 7.6 |
एन40एसएच | 12.5-12.8 | -0.11~-0.12 | ≥11.8 | ≥20 | -0.56~-0.70 | 38-41 | 150℃ | 7.6 |
एन42एसएच | 12.8-13.2 | -0.11~-0.12 | ≥12.4 | ≥20 | -0.56~-0.70 | 40-43 | 150℃ | 7.6 |
एन45एसएच | 13.2-13.8 | -0.11~-0.12 | ≥12.6 | ≥20 | -0.56~-0.70 | 43-46 | 150℃ | 7.6 |
N28UH | 10.2-10.8 | -0.11~-0.12 | ≥9.6 | ≥25 | -0.52~-0.70 | 26-29 | 180℃ | 7.6 |
N30UH | 10.8-11.3 | -0.11~-0.12 | ≥10.2 | ≥25 | -0.52~-0.70 | 28-31 | 180℃ | 7.6 |
N33UH | 11.3-11.7 | -0.11~-0.12 | ≥10.7 | ≥25 | -0.52~-0.70 | 31-34 | 180℃ | 7.6 |
N35UH | 11.8-12.2 | -0.11~-0.12 | ≥10.8 | ≥25 | -0.52~-0.70 | 33-36 | 180℃ | 7.6 |
N38UH | 12.2-12.5 | -0.11~-0.12 | ≥11.0 | ≥25 | -0.52~-0.70 | 36-39 | 180℃ | 7.6 |
N40UH | 12.5-12.8 | -0.11~-0.12 | ≥11.3 | ≥25 | -0.52~-0.70 | 38-41 | 180℃ | 7.6 |
N28EH | 10.4-10.9 | -0.105~-0.120 | ≥9.8 | ≥30 | -0.48~-0.70 | 26-29 | 200℃ | 7.6 |
N30EH | 10.8-11.3 | -0.105~-0.120 | ≥10.2 | ≥30 | -0.48~-0.70 | 28-31 | 200℃ | 7.6 |
N33EH | 11.3-11.7 | -0.105~-0.120 | ≥10.5 | ≥30 | -0.48~-0.70 | 31-34 | 200℃ | 7.6 |
N35EH | 11.7-12.2 | -0.105~-0.120 | ≥11.0 | ≥30 | -0.48~-0.70 | 33-36 | 200℃ | 7.6 |
N38EH | 12.2-12.5 | -0.105~-0.120 | ≥11.3 | ≥30 | -0.48~-0.70 | 36-39 | 200℃ | 7.6 |
N28AH | 10.4-10.9 | -0.105~-0.120 | ≥9.9 | ≥33 | -0.45~-0.70 | 26-29 | 230℃ | 7.6 |
N30AH | 10.8-11.3 | -0.105~-0.120 | ≥10.3 | ≥33 | -0.45~-0.70 | 28-31 | 230℃ | 7.6 |
N33AH | 11.3-11.7 | -0.105~-0.120 | ≥10.6 | ≥33 | -0.45~-0.70 | 31-34 | 230℃ | 7.6 |
टिप्पणी: · कार्यशील तापमान 20℃±2℃ के तहत, ऊपर के चुंबकीय मापदंडों और भौतिक गुणों का परीक्षण किया जाता है, जिसमें चुंबकीय बल की अपरिहार्य हानि 5% से अधिक नहीं होती है।· चुंबक का अधिकतम कार्यशील तापमान लंबाई और व्यास के अनुपात और पर्यावरणीय कारकों के कारण परिवर्तनशील होता है। . |
फ़ायदा:
इन चुम्बकों के गुण पारंपरिक चुम्बकों से कहीं बेहतर हैं और वे वर्तमान में उपयोग में सबसे शक्तिशाली हैं। उनका उच्च
ज़बरदस्ती और उच्च अवशेष नए डिज़ाइन और जहां स्थान सीमित है, वहां अनुप्रयोग के चुंबकीय क्षेत्र को बढ़ाने की संभावना की अनुमति देते हैं
या जहां एक मजबूत चुंबकीय क्षेत्र की आवश्यकता होती है।
एनडीएफईबी मैग्नेट जंग के प्रति बहुत संवेदनशील होते हैं। इसलिए एक सुरक्षात्मक सतह कोटिंग की आवश्यकता होती है। एनडीएफईबी चुंबक का उपयोग वातानुकूलित है
80ºC से 230ºC तक विस्तृत रेंज में तापमान द्वारा। और यह 0℃ से नीचे के तापमान पर भी काम करता है।
आवेदन पत्र:
नियोडिमियम मैग्नेट का उपयोग इलेक्ट्रॉनिक्स, ब्रेक सिस्टम में चार्ज कणों के फोकस, विक्षेपण के लिए विभिन्न प्रकार के चुंबकीय लेंस के रूप में किया जाता है।
ड्रिप, सेंसर, रोटर और माइक्रो मोटर्स में चुंबकीय प्रणाली, और विज्ञान, चिकित्सा (टोमोग्राफी, एनएमआर स्पेक्ट्रोमीटर), आदि का क्षेत्र।
आज पूरी दुनिया में NdFeB मैग्नेट का उपयोग बड़ी मात्रा में किया जाता है। इस सामग्री का विकास अभी पूरा नहीं हुआ है; अवशेष
और बलपूर्वक क्षेत्र की ताकत लगातार बढ़ाई जा रही है। एनडीएफईबी मैग्नेट की उच्च ऊर्जा का मतलब है कि मोटर और सेंसर बनाए जा सकते हैं
हमेशा छोटा - और यह प्रदर्शन दक्षता में वृद्धि का प्रतीक है। चल रहे सुधार इस दिलचस्प सामग्री को सतत बनाने में सक्षम बनाते हैं-
धीरे-धीरे नए क्षेत्रों में प्रवेश कराया गया।
सभी बताए गए मान IEC 60404-5 के अनुसार मानक नमूनों का उपयोग करके निर्धारित किए गए थे। निम्नलिखित विनिर्देश संदर्भ मान के रूप में कार्य करते हैं और
अलग हो सकता है। अधिक जानकारी के लिए कृपया हमारे एप्लिकेशन इंजीनियरों से संपर्क करें।